Concrete Waterproofing Compound
ApcoBuild Hydrotite IWC
  • Take Apco build Hydrotite IWC measured with a dispenser on the basis of 200 ml, per 50 kg bag of cement used
  • Mix it thoroughly in 15-20% of recommended water content for concrete mix and keep it ready, while other constituents of concrete / mortar are mixed with balance of 80-85% of the recommended water content.
  • ADD the Hydrotite IWC mixed in water to the above concrete / mortar mix and allow the wet mix for further 2 - 3 minutes resulting in a cohesive homogeneous mix etc.
  • Do not add ApcoBuild Hydrotite IWC to cement directly.
  • Maintain water-cement ratio as low as possible.
  • Do not increase the recommended dose.

  • Increases workability of concrete / mortar mix.
  • Does not effect setting time or strength.
  • Reduces capillary action yielding cohesive homogenous mix.
>Download Pdf Files For Terrace Water Proofing
More resources > > >
Disclaimer: These suggestions and data are based on information which we believe to be reliable. They are given for information only and in good faith, but without guarantee, as conditions and methods of use of our products are beyond our control. We recommend that the user determines the suitability of our materials and suggestions before adopting them on a commercial scale.